MSWI飞灰制阿利尼特复合水泥基材料的耐久性
1先进土木工程材料教育部重点实验室(同济大学)  2同济大学环境材料研究所
Durability of Composite Alinite Cement-based Materials from Municipal Solid Waste Incineration (MSWI) Fly Ash
1. Key Laboratory of Advanced Civil Engineering Materials, (Tongji University) Ministry of Education  2. Institute of environmental materials of Tongji University
下载:  PDF (1502KB) 
输出:  BibTeX | EndNote (RIS)      
摘要 以垃圾焚烧(MSWI)飞灰为主要原料,在实验室成功烧制了阿利尼特水泥熟料,基于此试验研究复合阿利尼特水泥基材料的耐久性。试样优选配比为阿利尼特水泥熟料:石膏:混合材(MSWI飞灰/粉煤灰/矿渣粉)=80%:5%:15%。结果表明:掺入混合材可增强阿利尼特水泥基材料的强抗硫酸盐侵蚀能力;不同混合材的掺入还可改善阿利尼特水泥基材料的抗渗性和抗碳化性能,改善幅度为试样AD3(掺15%矿渣粉)> AB3(掺15%MSWI飞灰)> AC3(掺15%粉煤灰);混合材的掺入对干缩性有负面影响。掺加15%MSWI飞灰的试样AB3,随着水化龄期增长,氯离子的溶出量呈降低趋势,且长龄期后溶出量渐趋稳定。
服务
把本文推荐给朋友
加入引用管理器
E-mail Alert
RSS
作者相关文章
郭晓潞
施惠生
关键词:  垃圾焚烧(MSWI)飞灰  阿利尼特水泥  抗压强度  耐久性    
Abstract:  Municipal solid waste incineration (MSWI) fly ash was successfully used as a main raw material in sintering and preparing alinite cement clinker in laboratory. Based on this, this work was focused on the durability composite alinite cement-based materials .The optimum mix mass ratio was that Alinite cement clinker: Gypsum: Cement additives (MSWI fly ash/ fly ash/slag) = 80%: 5%:15%. The experimental results showed that addition of cement additives could improve the resistance to sulfate attack of this alinite cement-based materials.The resistance to carbonation and water permeability could be improved by adding different type of cement additive. The effectiveness is specimen AD3 (with 15wt% slag) > AB3 (with 15wt% MSWI fly ash) > AC3 (with 15wt% fly ash). However, the addition of cement additives had negative effects on the dry shrinkage. Additionally, with the hydration ages increasing, the content of soluble chloride ion from alinite cement specimen AB3 was decreased. It would be stable in long term.
Key words:  municipal solid waste incineration (MSWI) fly ash    alinite cement    compressive strength    durability
收稿日期:  2013-01-18                出版日期:  2013-05-25      发布日期:  2018-06-01      整期出版日期:  2013-05-25
TQ172.18  
基金资助: 国家“863”计划(2006AA06Z363)项目、国家环保公益性行业科研专项(2012467026)
引用本文:    
郭晓潞, 施惠生, .
MSWI飞灰制阿利尼特复合水泥基材料的耐久性
[J]. 水泥技术, 2013, 1(3): 29-32.
GUO Xiao-lu, SHI Hui-sheng, .
Durability of Composite Alinite Cement-based Materials from Municipal Solid Waste Incineration (MSWI) Fly Ash
. Cement Technology, 2013, 1(3): 29-32.
链接本文:  
http://www.cemteck.com/CN/  或          http://www.cemteck.com/CN/Y2013/V1/I3/29
[1] 姚丕强, 韩辉, 俞为民. 新型低钙水泥的煅烧及初步应用研究[J]. 水泥技术, 2018, 1(2): 17-25.
[2] 宋留庆, 王峰, 聂文海, 柴星腾, 朱锋. 辊磨粉磨镍铁渣粉用作混凝土掺合料的性能研究[J]. 水泥技术, 2016, 1(2): 28-30.
[3] 郭晓潞, 施惠生, 董文靖. 纳米改性CFA-MSWI复合地聚合物的耐久性[J]. 水泥技术, 2014, 1(2): 30-34.
No Suggested Reading articles found!
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
    PDF Preview